Semi-hydraulic Lime

This is available as quick lime (lime obtained by calcining pure limestone) or as hydrated lime (dry power obtained by treating quick lime with water). The compressive strength of lime and mortar (1:3 by weight) should have 1.25 N/mm2 and 1.75 N/mm2 at 14 days and 28 days, respectively. This mortar is used for masonry work.